Analysis of the Effects of Lightning Strikes on Polymeric Composites[1]

By
Brian S. Hayes
Brian S. Hayes
Search for other works by this author on:
Luther M. Gammon
Luther M. Gammon
Search for other works by this author on:
Published:
2004
Publication history
February 26, 2011

Abstract

Lightning damage in polymer composites is manifested by damage at both the macroscopic or visual level and within the material microstructure. This article illustrates the effects of the laboratory-generated lightning strikes on polymeric composites.

You do not currently have access to this content.
Don't already have an account? Register

Brian S. Hayes, Luther M. Gammon, 2004. "Analysis of the Effects of Lightning Strikes on Polymeric Composites", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal