Skip to Main Content
ASM Handbook

Metallography and Microstructures

Edited by
George F. Vander Voort
George F. Vander Voort
Search for other works by this author on:
ASM International
Volume
9
ISBN electronic:
978-1-62708-177-1
Publication date:
2004
Book Chapter

Metallography and Microstructures of Titanium and Its Alloys

By
Luther M. Gammon
Luther M. Gammon
The Boeing Company
Search for other works by this author on:
Robert D. Briggs
Robert D. Briggs
The Boeing Company
Search for other works by this author on:
John M. Packard
John M. Packard
The Boeing Company
Search for other works by this author on:
Kurt W. Batson
Kurt W. Batson
The Boeing Company
Search for other works by this author on:
Rodney Boyer
Rodney Boyer
The Boeing Company
Search for other works by this author on:
Charles W. Domby
Charles W. Domby
The Boeing Company
Search for other works by this author on:
Published:
2004
Page range:
899 - 917
Publication history
November 01, 2004

Abstract

This article describes the fundamentals of titanium metallographic sample preparation. Representative micrographs are presented for each class of titanium alloys, including unalloyed titanium, alpha alloys, alpha-beta alloys, and beta titanium alloys. The article provides information on the macroexamination and microexamination for these alloys. It concludes with a discussion on the several metallographic techniques developed for specific purposes, such as recrystallization studies and microstructure/fracture topography correlations.

You do not currently have access to this content.
Don't already have an account? Register

Luther M. Gammon, Robert D. Briggs, John M. Packard, Kurt W. Batson, Rodney Boyer, Charles W. Domby, 2004. "Metallography and Microstructures of Titanium and Its Alloys", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal