Surface Degradation of Composites[1]

By
B.S. Hayes
B.S. Hayes
Search for other works by this author on:
L.M. Gammon
L.M. Gammon
Search for other works by this author on:
Published:
2004
Page range:
1 - 4
Publication history
February 26, 2011

Abstract

Polymer composite materials are subject to degradation if not appropriately protected from the environment. This article describes the effects of heat and atomic oxygen and ultraviolet-light on composite material surfaces, with illustrations.

You do not currently have access to this content.
Don't already have an account? Register

B.S. Hayes, L.M. Gammon, 2004. "Surface Degradation of Composites", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal