Skip to Main Content
ASM Handbook

Metallography and Microstructures

Edited by
George F. Vander Voort
George F. Vander Voort
Search for other works by this author on:
ASM International
Volume
9
ISBN electronic:
978-1-62708-177-1
Publication date:
2004
Book Chapter

Austenitic Manganese Steel Castings

By
Selçuk Kuyucak
Selçuk Kuyucak
Revising author
CANMET, Department of Natural Resources Canada
Search for other works by this author on:
Published:
2004
Page range:
701 - 708
Publication history
November 01, 2004

Abstract

This article focuses on the specimen preparation procedures of austenitic manganese steels: sectioning, mounting, and grinding. It provides information on macroexamination and microexamination of a fracture surface, the microstructure and special features of austenitic manganese steels, and the alloying elements used.

You do not currently have access to this content.
Don't already have an account? Register

Selçuk Kuyucak, 2004. "Austenitic Manganese Steel Castings", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal