Mounting of Specimens

Published:
2004
Page range:
242 - 256
Publication history
November 01, 2004

Abstract

Mounting of the specimen is often desirable or necessary for handling and metallographic polishing after the specimen is cut into an appropriate size. This article illustrates the different mechanical clamps used in mounting small specimens. It provides useful information on compression molded mounts, which are molded with thermoplastic and thermosetting resins. The article reviews several resins and their key factors, which help in the selection of the most appropriate mounting method and resin. It also discusses the characteristics of plastic mounting materials. The article provides information on the molds and resins used for castable mounts, vacuum treatment of mounts, special mount arrangements, and mount marking and storage.

You do not currently have access to this content.
Don't already have an account? Register

2004. "Mounting of Specimens", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal