Field Metallography Techniques

By
Bruce L. Bramfitt
Bruce L. Bramfitt
International Steel Group, Inc.
Search for other works by this author on:
Samuel J. Lawrence
Samuel J. Lawrence
International Steel Group, Inc.
Search for other works by this author on:
Published:
2004
Page range:
478 - 492
Publication history
November 01, 2004

Abstract

This article discusses the advantages and disadvantages of field metallography and describes the important material characteristics and other aspects to be considered before performing any metallographic procedure. It investigates the various stages of sample preparation in the metallographic laboratory: grinding, polishing, etching, preparing a replica, and obtaining a small sample. The article also illustrates the applications of field metallography with case studies.

You do not currently have access to this content.
Don't already have an account? Register

Bruce L. Bramfitt, Samuel J. Lawrence, 2004. "Field Metallography Techniques", Metallography and Microstructures, George F. Vander Voort