Microcrack Analysis of Composite Materials[1]

By
Brian S. Hayes
Brian S. Hayes
Search for other works by this author on:
Luther M. Gammon
Luther M. Gammon
Search for other works by this author on:
Published:
2004
Publication history
February 26, 2011

Abstract

This article describes the microcrack analysis of composite materials using bright-field illumination, polarized light, dyes, dark-field illumination, and epi-fluorescence.

You do not currently have access to this content.
Don't already have an account? Register

Brian S. Hayes, Luther M. Gammon, 2004. "Microcrack Analysis of Composite Materials", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal