Special Sample Preparation and Polishing for Fiber-Reinforced Composites[1]

By
Brian S. Hayes
Brian S. Hayes
Search for other works by this author on:
Luther M. Gammon
Luther M. Gammon
Search for other works by this author on:
Published:
2004
Publication history
February 26, 2011

Abstract

This article focuses on the sample preparation methods for titanium honeycomb composites, boron fiber composites, and titanium/polymeric composite hybrids. These include mounting, sectioning, grinding, and polishing. The article also provides information on the sample preparation of unstaged and staged prepreg materials for optical analysis.

You do not currently have access to this content.
Don't already have an account? Register

Brian S. Hayes, Luther M. Gammon, 2004. "Special Sample Preparation and Polishing for Fiber-Reinforced Composites", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal