Abstract

This article provides information on the general structural features and origins of metals. The characteristic structural features of single-phase metals and alloys, such as grain structure and substructure, are discussed. The article also describes the major types of multiphase structures and macrostructure of metals and alloys.

You do not currently have access to this content.
Don't already have an account? Register

2004. "Introduction to Structures in Metals", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal