Metallography and Microstructures of Magnesium and Its Alloys

By
Toby V. Padfield
Toby V. Padfield
ZF Sachs Automotive of America
Search for other works by this author on:
Published:
2004
Page range:
801 - 815
Publication history
November 01, 2004

Abstract

Magnesium and its alloys are among the most difficult metals to prepare for metallographic examination. This article describes specimen preparation processes, including sectioning, mounting, grinding, and polishing. It discusses macro and microexamination techniques as well as related etching processes, including macroetching and color etching based on polarized light enhancement. The article concludes with an overview of the effects of alloying elements, including aluminum, beryllium, calcium, copper, iron, lithium, manganese, rare earth metals, silicon, silver, strontium, thorium, tin, zinc, and zirconium.

You do not currently have access to this content.
Don't already have an account? Register

Toby V. Padfield, 2004. "Metallography and Microstructures of Magnesium and Its Alloys", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal