Metallography of Biomedical Orthopedic Alloys

By
D.J. Medlin
D.J. Medlin
Zimmer, Inc.
Search for other works by this author on:
R. Compton
R. Compton
Zimmer, Inc.
Search for other works by this author on:
Published:
2004
Page range:
961 - 968
Publication history
November 01, 2004

Abstract

Metallography plays a significant role in the quality control of metals and alloys used in the manufacture of implantable surgical devices. This article provides information and data on metallographic techniques along with images showing the microstructure of biomedical orthopedic alloys, including stainless steels, cobalt-base alloys, titanium and titanium alloys, porous coatings, and emerging materials.

You do not currently have access to this content.
Don't already have an account? Register

D.J. Medlin, R. Compton, 2004. "Metallography of Biomedical Orthopedic Alloys", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal