Skip to Main Content
ASM Handbook

Metallography and Microstructures

Edited by
George F. Vander Voort
George F. Vander Voort
Search for other works by this author on:
ASM International
Volume
9
ISBN electronic:
978-1-62708-177-1
Publication date:
2004
Book Chapter

Introduction to Transformation Structures

By
Arnold R. Marder
Arnold R. Marder
Department of Materials Science and Engineering, Lehigh University
Search for other works by this author on:
Published:
2004
Page range:
132 - 133
Publication history
November 01, 2004

Abstract

This introductory article provides basic information on the various aspects of solid-state transformation: multiphase microstructures, substructures, and crystallography, which assist in characterizing the morphology of phase transformations. It contains a flowchart that illustrating the classification of transformations by growth processes.

You do not currently have access to this content.
Don't already have an account? Register

Arnold R. Marder, 2004. "Introduction to Transformation Structures", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal