Microstructural Characterization of Thermal Spray Coatings

By
J.R. Davis
J.R. Davis
Davis & Associates
Search for other works by this author on:
Published:
2004
Page range:
1038 - 1046
Publication history
November 01, 2004

Abstract

This article reviews how process variations influence the characteristics of thermal spray coatings. It describes various specimen preparation techniques, which allow accurate microstructural analysis. These techniques include sectioning, cleaning, mounting, planar grinding, fine grinding, rough polishing, and etching. The article provides information on the problems associated with specimen preparation. It concludes with a discussion on the various methods of analysis for thermal spray coatings.

You do not currently have access to this content.
Don't already have an account? Register

J.R. Davis, 2004. "Microstructural Characterization of Thermal Spray Coatings", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal