Skip to Main Content
ASM Handbook

Metallography and Microstructures

Edited by
George F. Vander Voort
George F. Vander Voort
Search for other works by this author on:
ASM International
Volume
9
ISBN electronic:
978-1-62708-177-1
Publication date:
2004
Book Chapter

Metallography and Microstructures of Semisolid Formed Alloys

By
Edward J. Vinarcik
Edward J. Vinarcik
Search for other works by this author on:
Published:
2004
Page range:
1021 - 1037
Publication history
November 01, 2004

Abstract

This article begins with a description of indirect and direct semisolid metalworking processes. It then provides information on alloy compositions of common aluminum semisolid metalworking alloys and primary die-cast magnesium alloys in a tabular form. The article describes the macroscopic examination of defects, which occur in semisolid metalworking with illustrations. It discusses the macroscopic examination of gating systems and semisolid feedstocks. The article also provides information on feedstock microstructures, direct semisolid metalworking component microstructures, and indirect semisolid metalworking component microstructures of series 300 aluminum casting alloys and magnesium die-casting alloys.

You do not currently have access to this content.
Don't already have an account? Register

Edward J. Vinarcik, 2004. "Metallography and Microstructures of Semisolid Formed Alloys", Metallography and Microstructures, George F. Vander Voort

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal