Abstract

This article provides a discussion on binary alloy phase diagrams published in this handbook. All diagrams presented are for stable equilibrium conditions, except where metastable conditions are indicated.

Abstract

This article is a compilation of binary alloy phase diagrams for which silver (Ag) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.

Abstract

This article is a compilation of binary alloy phase diagrams for which aluminum (Al) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system, a table of crystallographic data is provided that includes the composition, Pearson symbol, space group, and prototype for each phase.

You do not currently have access to this content.
Don't already have an account? Register

2016. "Binary Phase Diagrams", Alloy Phase Diagrams, H. Okamoto, M.E. Schlesinger, E.M. Mueller

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal