Skip to Main Content
ASM Handbook

Alloy Phase Diagrams

Edited by
H. Okamoto
H. Okamoto
Search for other works by this author on:
M.E. Schlesinger
M.E. Schlesinger
Search for other works by this author on:
E.M. Mueller
E.M. Mueller
Search for other works by this author on:
ASM International
Volume
3
ISBN electronic:
978-1-62708-163-4
Publication date:
2016
Book Chapter

Ge (Germanium) Ternary Alloy Phase Diagrams

Published:
2016
Page range:
741 - 741
Publication history
June 02, 2016

Abstract

This article is a compilation of ternary alloy phase diagrams for which germanium (Ge) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes phase diagram of Ge-Sb-Te liquidus projection.

You do not currently have access to this content.
Don't already have an account? Register

2016. "Ge (Germanium) Ternary Alloy Phase Diagrams", Alloy Phase Diagrams, H. Okamoto, M.E. Schlesinger, E.M. Mueller

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal