Skip to Main Content
ASM Handbook

Alloy Phase Diagrams

Edited by
H. Okamoto
H. Okamoto
Search for other works by this author on:
M.E. Schlesinger
M.E. Schlesinger
Search for other works by this author on:
E.M. Mueller
E.M. Mueller
Search for other works by this author on:
ASM International
Volume
3
ISBN electronic:
978-1-62708-163-4
Publication date:
2016
Book Chapter

Fe (Iron) Ternary Alloy Phase Diagrams

Published:
2016
Page range:
737 - 740
Publication history
June 02, 2016

Abstract

This article is a compilation of ternary alloy phase diagrams for which iron (Fe) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Fe-Mn-Ni liquidus projection; Fe-Mn-Ni isothermal section at 750 °C; Fe-Mn-Ni isothermal section at 850 °C; Fe-Mn-Ni isothermal section at 650 °C; Fe-Mn-Ni isothermal section at 550 °C; Fe-Mo-Nb isothermal section at 1050 °C; Fe-Mo-Nb isothermal section at 1150 °C; Fe-Mo-Nb isothermal section at 900 °C; Fe-Mo-Ni liquidus projection; Fe-Mo-Ni isothermal section at 1100 °C; Fe-Mo-Ni isothermal section at 1200 °C; Fe-Ni-W liquidus and solidus projections; Fe-Ni-W isothermal section at 1500 °C; Fe-Ni-W isothermal section at 1455 °C; Fe-Ni-W isothermal section at 1465 °C; and Fe-Ni-W isothermal section at 1400 °C.

You do not currently have access to this content.
Don't already have an account? Register

2016. "Fe (Iron) Ternary Alloy Phase Diagrams", Alloy Phase Diagrams, H. Okamoto, M.E. Schlesinger, E.M. Mueller

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal