Flanging is a process used to form a projecting rim or edge on a part. This article explores how to determine aluminum flanging limits in terms of fracture, wrinkling, and springback, and their influencing material and process parameters with examples.

You do not currently have access to this content.
Don't already have an account? Register

Jian Cao, 2006. "Flanging of Aluminum", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal