Book Chapter

Selection and Use of Lubricants in Forming of Sheet Metal

Published:
2006
Page range:
248 - 264
Publication history
August 14, 2006

Abstract

This article provides an overview of the interfacial interactions with a lubricant film between a die and a metal, lubricant mechanisms, chemistry, qualification testing, application methods, and property test methods. It focuses on sheet metal-forming operations, although the discussions are relevant to metal-forming operations in general. The article also deals with lubricant selection as influenced by the metal to be formed and particular sheet-metal forming operations. The article also discusses some aspects of microbiology and toxicity in lubricants.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Selection and Use of Lubricants in Forming of Sheet Metal", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal