Forming of Steel Strip in Multiple-Slide Machines

Published:
2006
Page range:
554 - 561
Publication history
August 22, 2006

Abstract

Multiple-slide forming is a process in which the workpiece is progressively formed in a combination of units that can be used in various ways for the automated fabrication of a large variety of simple and intricately shaped parts from coil stock or wire. This article discusses the components of multiple-slide rotary forming machines involved in the blanking and forming of strip stock. It describes a complicated application of the two-level forming, with an example.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Forming of Steel Strip in Multiple-Slide Machines", Metalworking: Sheet Forming, S.L. Semiatin