Rubber-Pad Forming and Hydroforming

Published:
2006
Page range:
375 - 385
Publication history
August 16, 2006

Abstract

This article focuses on the three basic groups of flexible-die forming methods: rubber pad, fluid cell, and fluid forming. It provides information on the Guerin process, the Verson-Wheelon process, the trapped-rubber process, the Marform process, the Hydroform process, the SAAB process, and the Demarest process. The article provides a discussion on the procedures of these processes, as well as the presses and tools used. It describes the methods of hydraulic forming of thin metal parts, namely, hydraulic forming with diaphragm, hydraulic forming with gasket and pressure control, and hydrobuckling.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Rubber-Pad Forming and Hydroforming", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal