Flattening, Leveling, Slitting, and Shearing of Coiled Product

By
L. Chen
L. Chen
Technical Materials, Inc.
Search for other works by this author on:
Published:
2006
Page range:
46 - 56
Publication history
August 08, 2006

Abstract

Metal production mills produce flat metal sheet and strip products into coil forms that are subjected to further fabrication for shape correction. This article provides a discussion on the principle of shape correction and describes the role of various fabrication processes in shape correction. These processes include flattening, leveling, slitting, and cut-to-length.

You do not currently have access to this content.
Don't already have an account? Register

L. Chen, 2006. "Flattening, Leveling, Slitting, and Shearing of Coiled Product", Metalworking: Sheet Forming, S.L. Semiatin