Skip to Main Content
ASM Handbook

Metalworking: Sheet Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14B
ISBN electronic:
978-1-62708-186-3
Publication date:
2006
Book Chapter

Stretch Forming

By
Mahmoud Y. Demeri
Mahmoud Y. Demeri
Revising author
FormSys, Inc.
Search for other works by this author on:
Published:
2006
Page range:
337 - 344
Publication history
August 16, 2006

Abstract

Stretch forming is the forming of sheet, bars, and rolled or extruded sections over a die or form block of the required shape while the workpiece is held in tension. This article discusses the applicability, advantages, and machines and accessories of stretch forming. It provides a detailed discussion on four methods of stretch forming, namely, stretch draw forming, stretch wrapping, compression forming, and radial draw forming.

You do not currently have access to this content.
Don't already have an account? Register

Mahmoud Y. Demeri, 2006. "Stretch Forming", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal