Forming of Wire

By
David Berardis
David Berardis
Revising author
Fenn Technologies
Search for other works by this author on:
Published:
2006
Page range:
487 - 491
Publication history
August 22, 2006

Abstract

This article describes the operation procedures of wire rolling in a Turks Head machine. It discusses spring coiling, as well as the manual and power bending used in the wire forming process. The article contains a table that lists examples of several wire-forming production problems and solutions. Lubricants for wire forming such as inorganic fillers, soluble oils, and boundary lubricants are reviewed. The article also analyzes the applications of lubricants in wire forming.

You do not currently have access to this content.
Don't already have an account? Register

David Berardis, 2006. "Forming of Wire", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal