Trimming Operations

Published:
2006
Page range:
69 - 73
Publication history
August 08, 2006

Abstract

Trimming is the removal of excess metal from a stamped part to allow the part to reach the finished stage or to prepare it for subsequent operations. This article presents an analysis of parts to be trimmed and describes the selection criteria for the different types of trimming dies such as conventional trimming dies and cam trimming dies. It provides information on rough and finish trimming and construction details of trimming dies. The article reviews the selection criteria of presses for a trimming operation. It provides a discussion on the scrap and material handling processes in trimming.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Trimming Operations", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal