Formability Testing of Sheet Metals

By
Michael Miles
Michael Miles
Revising author
Brigham Young University
Search for other works by this author on:
Published:
2006
Page range:
673 - 696
Publication history
August 28, 2006

Abstract

Sheet metal forming operations are so diverse in type, extent, and rate that no single test provides an accurate indication of the formability of a material in all situations. This article presents an overview of types of forming, formability problems, and principal methods of measuring deformation. It reviews the effect of materials properties and temperature on formability. The article provides a detailed discussion on the two major categories of formability tests such as the intrinsic test, including uniaxial tension testing, plane-strain tension testing, biaxial stretch testing, and simulative tests such as bending tests, stretching tests, the Ohio State University test, the drawing test, and stretch-drawing tests. It extends the correlation between simulative tests and materials properties using forming limit diagrams and circle grid analysis, and discusses the improvements to the forming limit diagram technology.

You do not currently have access to this content.
Don't already have an account? Register

Michael Miles, 2006. "Formability Testing of Sheet Metals", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal