Skip to Main Content
ASM Handbook

Metalworking: Sheet Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14B
ISBN electronic:
978-1-62708-186-3
Publication date:
2006
Book Chapter

Incremental Sheet Forming[1]

By
G. Hirt
G. Hirt
RWTH Aachen University
Search for other works by this author on:
M. Bambach
M. Bambach
RWTH Aachen University
Search for other works by this author on:
Published:
2006
Publication history
September 05, 2012

Abstract

This article provides an overview of the incremental sheet forming (ISF) process and discusses the process variations of ISF. These variations include single-point incremental forming, two-point incremental forming, and kinematic incremental sheet forming. The article discusses the machines and equipment used in the process and describes the process parameters, process mechanics, and process limits. It illustrates multistage forming strategies and summarizes difficulties that exist with regard to the finite-element process simulation of ISF process. The article also describes hybrid process variations, such as stretch forming and laser-assisted ISF.

You do not currently have access to this content.
Don't already have an account? Register

G. Hirt, M. Bambach, 2006. "Incremental Sheet Forming", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal