Die Manufacture by Electrical Discharge Machining

Published:
2006
Page range:
280 - 286
Publication history
August 14, 2006

Abstract

The electrical discharge machining (EDM) process is used for machining dies because of its ability to machining difficult geometries or materials with poor machinability. This article provides a discussion on the fundamentals of electrical discharge erosion and the principles of EDM and orbital-movement EDM. It discusses various aspects of wire EDM in machining dies and provides an overview of the materials used in EDM electrodes. The article concludes with a discussion on electrochemical machining.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Die Manufacture by Electrical Discharge Machining", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal