Skip to Main Content
ASM Handbook

Metalworking: Sheet Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14B
ISBN electronic:
978-1-62708-186-3
Publication date:
2006
Book Chapter

Indirect Nondestructive Measurements of Die Wear in Stamping Productions[1]

By
Huimin Liu
Huimin Liu
Materials Surface Engineering and Testing, Ford Motor Company
[2]
Search for other works by this author on:
Sriram Sadagopan
Sriram Sadagopan
Mittal Steel USA R&D
Search for other works by this author on:
Published:
2006
Publication history
March 09, 2009

Abstract

The measurement techniques for die wear can be classified into the following two categories: direct measurements, which are done using lab techniques; and indirect nondestructive measurements, which are done by plant monitoring. This article describes the details of the plant monitoring techniques, along with comprehensive discussions on the measured wear data based on roughness and hardness of die surfaces. It presents a comparison between the predicted and measured die wear rates.

You do not currently have access to this content.
Don't already have an account? Register

Huimin Liu, Sriram Sadagopan, 2006. "Indirect Nondestructive Measurements of Die Wear in Stamping Productions", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal