Selection of Materials for Shearing, Blanking, and Piercing Tools

Published:
2006
Page range:
57 - 68
Publication history
August 08, 2006

Abstract

Shearing is a process of cutting flat product with blades, rotary cutters, or with the aid of a blanking or punching die. This article commences with a description of some wear and material factors for tools used to shear flat product, principally sheet. Methods of wear control are reviewed in terms of tool materials, coatings and surface treatments, and lubrication. The article discusses tool steels that are used for cold and hot shearing, and rotary slitting. It provides information on the materials used for two main categories of machine knives: circular knives and straight knife cutters. The article also discusses the selection of materials for blanking and piercing dies and provides examples that illustrate the various types of tooling changes for blanking high-carbon steel.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Selection of Materials for Shearing, Blanking, and Piercing Tools", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal