Abstract
This article describes the operation procedures of wire rolling in a Turks Head machine. It discusses spring coiling, as well as the manual and power bending used in the wire forming process. The article contains a table that lists examples of several wire-forming production problems and solutions. Lubricants for wire forming such as inorganic fillers, soluble oils, and boundary lubricants are reviewed. The article also analyzes the applications of lubricants in wire forming.
You do not currently have access to this content.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InDavid Berardis, 2006. "Forming of Wire", Metalworking: Sheet Forming, S.L. Semiatin
Download citation file:
×
Advertisement
Mager
Mager Scientific is your exclusive source for Qness hardness testing equipment in the United States.