Straightening of Tubing

Published:
2006
Page range:
483 - 486
Publication history
August 21, 2006

Abstract

Tubing of any cross-sectional shape can be straightened by using various equipment and techniques. This article provides a discussion on principal factors that influence the procedures and tooling of tube straightening. It describes the tooling and application of different types of tube straightening techniques, namely, press straightening, parallel-roll straightening, two-roll rotary straightening, multiple-roll rotary straightening, and ovalizing in rotary straighteners.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Straightening of Tubing", Metalworking: Sheet Forming, S.L. Semiatin