Straightening of Bars, Shapes, and Long Parts

Published:
2006
Page range:
472 - 482
Publication history
August 21, 2006

Abstract

Bars, structural shapes, and long parts are straightened by bending, twisting, or stretching. This article describes the straightening of bars, shapes, and long parts by material displacement, heating, and presses. It explains the process of parallel-roll straightening, automatic press roll straightening, moving-insert straightening, parallel-rail straightening, and epicyclic straightening. The article concludes with a discussion on straightening in bar production.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Straightening of Bars, Shapes, and Long Parts", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal