Forming of Steel Tailor-Welded Blanks[1]

Published:
2006
Page range:
539 - 546
Publication history
August 22, 2006

Abstract

This article briefly reviews the forming of steel tailor-welded blanks (TWB) with a discussion on the effects of welding on forming. It presents the parameters that are monitored to control the stamping operation for tailor-welded blanks. The article discusses weld factors such as the orientation of weld relative to metal movement in dies, the formability of TWB materials, die and press considerations, and specific factors for the drawing, stretching, and bending of steel tailor-welded blanks.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Forming of Steel Tailor-Welded Blanks", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal