Book Chapter

Blanking and Piercing of Electrical Steel Sheet

Published:
2006
Page range:
171 - 176
Publication history
August 10, 2006

Abstract

This article discusses the presses, auxiliary equipment, and dies used in the blanking and piercing of commonly used magnetically soft materials, namely, low-carbon electrical steels and oriented and nonoriented silicon electrical steels. It describes the effect of stock thickness and work metal composition and condition on blanking and piercing. The article provides an overview of the influence of burr height on stacking factors and presents a discussion on the lubrication and core plating of electrical steels that ease the process.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Blanking and Piercing of Electrical Steel Sheet", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal