Useful Formulas for Deformation Analysis and Workability Testing

Published:
2006
Page range:
887 - 891
Publication history
September 04, 2006

Abstract

This article presents formulas for calculating the following: effective stress, strain, and strain rate (isotropic material) in arbitrary coordinates and in principal coordinates; compression testing, tension testing, and torsion testing of isotropic material; and Barlat's anisotropic yield function Yld2000-2d for plane-stress deformation of sheet material. It also contains formulas related to flat (sheet) rolling, conical-die extrusion, wire drawing, bending, and deep drawing of cups from sheet metal.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Useful Formulas for Deformation Analysis and Workability Testing", Metalworking: Sheet Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal