The four-point method to estimate fatigue life behavior from tensile properties allows the construction of fatigue life curves from more readily available handbook data. This article provides information on the strain-based four-point method and the stress-based four-point method. The effects of mean stress or strain on transition fatigue life are reviewed. The article describes the determination of four fatigue-life parameters either by curve fitting actual fatigue life test data or approximating the constants from tensile properties. It contains a table that lists the tensile properties of various alloys.

You do not currently have access to this content.
Don't already have an account? Register

1996. "Parameters for Estimating Fatigue Life", Fatigue and Fracture

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal