Skip to Main Content
ASM Handbook

Fatigue and Fracture

ASM International
Volume
19
ISBN electronic:
978-1-62708-193-1
Publication date:
1996
Book Chapter

Elevated-Temperature Crack Growth

By
Richard H. Norris
Richard H. Norris
Mechanical Properties Research Laboratory, School of Materials Science and Engineering, Georgia Institute of Technology
Search for other works by this author on:
Parmeet S. Grover
Parmeet S. Grover
Mechanical Properties Research Laboratory, School of Materials Science and Engineering, Georgia Institute of Technology
Search for other works by this author on:
B. Carter Hamilton
B. Carter Hamilton
Mechanical Properties Research Laboratory, School of Materials Science and Engineering, Georgia Institute of Technology
Search for other works by this author on:
Ashok Saxena
Ashok Saxena
Mechanical Properties Research Laboratory, School of Materials Science and Engineering, Georgia Institute of Technology
Search for other works by this author on:
Published:
1996
Page range:
507 - 519

Abstract

This article describes the concepts for characterizing and predicting elevated-temperature crack growth in structural materials. It discusses both creep and creep-fatigue crack growth and focuses mainly on creep crack growth tests that are carried out in accordance with ASTM E 1457. The article provides information on typical test procedures and equipment used for these tests. It concludes with information on crack growth correlations.

You do not currently have access to this content.
Don't already have an account? Register

Richard H. Norris, Parmeet S. Grover, B. Carter Hamilton, Ashok Saxena, 1996. "Elevated-Temperature Crack Growth", Fatigue and Fracture

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal