Behavior of Small Fatigue Cracks

By
R. Craig McClung
R. Craig McClung
Southwest Research Institute
Search for other works by this author on:
Kwai S. Chan
Kwai S. Chan
Southwest Research Institute
Search for other works by this author on:
Stephen J. Hudak, Jr.
Stephen J. Hudak, Jr.
Southwest Research Institute
Search for other works by this author on:
David L. Davidson
David L. Davidson
Southwest Research Institute
Search for other works by this author on:
Published:
1996
Page range:
153 - 158

Abstract

This article defines different types of small cracks and identifies the different factors that influence small-crack behavior. Appropriate analysis techniques, including both rigorous scientific and practical engineering treatments, are briefly described. Important material data issues are addressed, including increased scatter in small-crack data and recommended small-crack test methods. The article highlights the applications where small cracks may be particularly important.

You do not currently have access to this content.
Don't already have an account? Register

R. Craig McClung, Kwai S. Chan, Stephen J. Hudak, Jr., David L. Davidson, 1996. "Behavior of Small Fatigue Cracks", Fatigue and Fracture