Fretting Fatigue

By
S.J. Shaffer
S.J. Shaffer
Battelle Memorial Institute
Search for other works by this author on:
W.A. Glaeser
W.A. Glaeser
Battelle Memorial Institute
Search for other works by this author on:
Published:
1996
Page range:
321 - 330

Abstract

Fretting is a special wear process that occurs at the contact area between two materials under load and subject to slight relative movement by vibration or some other force. This article focuses on measures to avoid or minimize crack initiation and fretting fatigue. It lists the factors that are known to influence the severity of fretting and discusses the variables that contribute to shear stresses. These variables include normal load, relative displacement (slip amplitude), and coefficient of friction. The article describes the general geometries and loading conditions for fretting fatigue. It presents the types of fretting fatigue tests and the effect of variables on fretting fatigue from different research test programs. The article also lists the general principles and practical methods for the abatement or elimination of fretting fatigue.

You do not currently have access to this content.
Don't already have an account? Register

S.J. Shaffer, W.A. Glaeser, 1996. "Fretting Fatigue", Fatigue and Fracture

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal