Abstract

This article discusses the various options for controlling fatigue and fractures in welded steel structures, with illustrations. It describes the factors that influence them the most. The article details some of the leading codes and standards for designing against failure mechanisms. Codes are presented for fitness-for-service and standards for fatigue and fracture control.

You do not currently have access to this content.
Don't already have an account? Register

Tarsem Jutla, 1996. "Fatigue and Fracture Control of Weldments", Fatigue and Fracture

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal