Abstract

This article discusses the conditions for collapse in center-cracked panels and describes the energy criterion for fracture. Measurement of toughness of any material by means of tensile and crack test is discussed. The procedures to be followed for linear elastic fracture mechanics cases are reviewed, along with elastic-plastic fracture mechanics and plastic fracture mechanics procedures with the aid of residual strength diagram. The article also explains the geometry factors needed to determine the toughness of materials.

You do not currently have access to this content.
Don't already have an account? Register

David Broek, 1996. "Residual Strength of Metal Structures", Fatigue and Fracture

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal