Fatigue and Fracture Resistance of Heat-Resistant (Cr-Mo) Ferritic Steels

By
R.W. Swindeman
R.W. Swindeman
Oak Ridge National Laboratory
Search for other works by this author on:
W. Ren
W. Ren
Oak Ridge National Laboratory
Search for other works by this author on:
Published:
1996
Page range:
704 - 711

Abstract

Cr-Mo steels are preferred in the construction of high-temperature components because they possess excellent strength, toughness, and corrosion resistance relative to carbon steels and most low-alloy steels. This article discusses the composition and metallurgy of the heat-resistant Cr-Mo steels. It details the Charpy V-notch (CVN) toughness properties of Cr-Mo steels relevant to fatigue and fracture resistance. The fracture mechanics of Cr-Mo steels are reviewed. The article analyzes the characterization of low-cycle fatigue based on fatigue damage calculations. It concludes with information on fatigue crack growth and fatigue behavior of weldments.

You do not currently have access to this content.
Don't already have an account? Register

R.W. Swindeman, W. Ren, 1996. "Fatigue and Fracture Resistance of Heat-Resistant (Cr-Mo) Ferritic Steels", Fatigue and Fracture, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal