Fatigue and Fracture of Nickel-Base Superalloys

By
Bruce F. Antolovich
Bruce F. Antolovich
Metallurgical Research Consultants, Inc.
Search for other works by this author on:
Published:
1996
Page range:
854 - 868

Abstract

This article discusses fracture, fatigue, and creep of nickel-base superalloys with additional emphasis on directionally solidified and single-crystal applications. It analyzes the physical metallurgy of these alloys. The effects of grain boundary and grain size on failure are summarized. The article also discusses the effects of microstructure and extrinsic parameters on fatigue crack propagation (FCP). It details the modeling of FCP rates and creep and creep-fatigue crack growth rates.

You do not currently have access to this content.
Don't already have an account? Register

Bruce F. Antolovich, 1996. "Fatigue and Fracture of Nickel-Base Superalloys", Fatigue and Fracture, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal