Fatigue Failure in Metals[1]

By
Morris E. Fine
Morris E. Fine
R.R. McCormick School of Engineering & Applied Science, Department of Materials Science & Engineering, Northwestern University
Search for other works by this author on:
Yip-Wah Chung
Yip-Wah Chung
R.R. McCormick School of Engineering & Applied Science, Department of Materials Science & Engineering, Northwestern University
Search for other works by this author on:
Published:
1996
Page range:
63 - 72

Abstract

Fatigue damage in metals is caused by the simultaneous action of cyclic stress, tensile stress, and plastic strain. This article details the fundamental aspects of the stages of the fatigue failure process. These include cyclic plastic deformation prior to fatigue crack initiation, initiation of one or more microcracks, propagation or coalescence of microcracks to form one or more microcracks, and propagation of one or more macrocracks.

You do not currently have access to this content.
Don't already have an account? Register

Morris E. Fine, Yip-Wah Chung, 1996. "Fatigue Failure in Metals", Fatigue and Fracture, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal