Contact Fatigue

By
W.A. Glaeser
W.A. Glaeser
Battelle Laboratories
Search for other works by this author on:
S.J. Shaffer
S.J. Shaffer
Battelle Laboratories
Search for other works by this author on:
Published:
1996
Page range:
331 - 336

Abstract

Contact fatigue is a surface-pitting-type failure commonly found in ball or roller bearings. This article discusses the mechanisms of contact fatigue found in gears, cams, valves, rails, and gear couplings. It discusses the statistical analysis of rolling contact bearing-life tests. The article concludes with information on various approaches that improve the contact fatigue resistance of rolling contact systems.

You do not currently have access to this content.
Don't already have an account? Register

W.A. Glaeser, S.J. Shaffer, 1996. "Contact Fatigue", Fatigue and Fracture, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal