Book Chapter

Fatigue Properties in Engineering

By
D.W. Cameron
D.W. Cameron
Allegany, NY
Search for other works by this author on:
D.W. Hoeppner
D.W. Hoeppner
Department of Mechanical Engineering, University of Utah
Search for other works by this author on:
Published:
1996
Page range:
15 - 26

Abstract

Fatigue properties are an integral part of materials comparison activities and offer information for structural life estimation in many engineering applications. This article presents three general approaches to fatigue design, with a discussion on their respective attributes. These include infinite-life criterion, finite-life criterion, and damage tolerant criterion. The article describes the individual property requirements of these approaches. It also presents selected examples of properties that reflect some detail of these approaches.

You do not currently have access to this content.
Don't already have an account? Register

D.W. Cameron, D.W. Hoeppner, 1996. "Fatigue Properties in Engineering", Fatigue and Fracture, ASM Handbook Committee