Skip to Main Content
ASM Handbook

Fatigue and Fracture

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
19
ISBN electronic:
978-1-62708-193-1
Publication date:
1996
Book Chapter

Fatigue Properties of Copper Alloys

By
Jack Crane
Jack Crane
Consultant
Search for other works by this author on:
John O. Ratka
John O. Ratka
Brush Wellman
Search for other works by this author on:
John F. Breedis
John F. Breedis
Olin Brass
Search for other works by this author on:
Published:
1996
Page range:
869 - 873

Abstract

Copper alloys are classified by the International Unified Numbering System designations to identify alloy groups by major alloying element. This article presents the designations and compositions of various copper alloys, such as brasses, nickel silvers, bronzes, beryllium coppers, and spinodal alloys. It discusses the fatigue testing of the copper alloys and tabulates the tensile and fatigue strengths of the copper alloys. The article schematically illustrates S-N curves for the solid-solution (non-aging) strengthened alloys. It concludes with a discussion on the role of microstructure in the fatigue performance of beryllium copper alloys.

You do not currently have access to this content.
Don't already have an account? Register

Jack Crane, John O. Ratka, John F. Breedis, 1996. "Fatigue Properties of Copper Alloys", Fatigue and Fracture, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal