Fatigue damage in metals is caused by the simultaneous action of cyclic stress, tensile stress, and plastic strain. This article details the fundamental aspects of the stages of the fatigue failure process. These include cyclic plastic deformation prior to fatigue crack initiation, initiation of one or more microcracks, propagation or coalescence of microcracks to form one or more microcracks, and propagation of one or more macrocracks.

Abstract

This article discusses the microstructural processes that take place during plastic deformation and presents a plain phenomenological and general description of the cyclic stress-strain (CSS) response. It emphasizes the microstructural aspects of cyclic loading on single-phase materials tested in initially soft, dislocation-poor conditions resulting from a prior heat treatment. The article discusses deformation-induced phase transformations in austenitic stainless steels and commercial age-hardened aluminum alloys. It describes the interaction of dislocations and the strengthening of second-phase particles. The article also provides a description of the framework used to model the CSS response on a physical basis.

You do not currently have access to this content.
Don't already have an account? Register

1996. "Fatigue Mechanisms, Crack Growth, and Testing", Fatigue and Fracture, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal