Gear Manufacture

By
Theodore J. Krenzer
Theodore J. Krenzer
Revising author
The Gleason Works, Division of Gleason Corporation
Search for other works by this author on:
Joseph W. Coniglio
Joseph W. Coniglio
Revising author
Gould & Eberhardt Gear Machinery Corporation
Search for other works by this author on:
Published:
1989
Page range:
330 - 355

Abstract

This article discusses the different classes of gears, namely, spur, helical, herringbone, crossed-axes helical, worm, internal, rack, bevel, or face-type. It describes the methods used to cut the teeth of gears other than bevel gears: milling, broaching, shear cutting, hobbing, shaping, and rack cutting. The article also reviews the methods that are used to cut the teeth of bevel gears, such as face mill cutting, face hob cutting, formate cutting, helix form cutting, the Cyclex method, and template machining. The machining methods best suited to specific conditions are discussed. The article presents the factors influencing the choice of cutting speed and cutting fluids. It outlines two basic methods for the grinding of gear teeth: form grinding and generation grinding. The article concludes with information on the gear inspection techniques used to determine whether the resulting product meets design specifications and requirements.

You do not currently have access to this content.
Don't already have an account? Register

Theodore J. Krenzer, Joseph W. Coniglio, 1989. "Gear Manufacture", Machining

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal